Fatigue Fracture
fatigue_fractureCompute Mode-I stress intensity factors, critical crack sizes, and fatigue crack growth for plates and specimens using LEFM, with geometry/yield checks and Paris/Forman integration.
Instructions
Mode-I LEFM: infinite/finite plates, edge/double-edge, Newman-Raju surface tension, ASTM E399 SENB/CT factors. K, critical crack, Irwin zones and size screen; Paris/Forman growth with adaptive integration and threshold. Geometry/yield limits enforced; no retardation or closure model.
Tool call template
This tool declares no required parameters. Add optional parameters from the input schema as needed.
{
"id": 1,
"jsonrpc": "2.0",
"method": "tools/call",
"params": {
"arguments": {},
"name": "fatigue_fracture"
}
}Input Schema
| Name | Required | Description | Default |
|---|---|---|---|
| load | No | Maximum applied force P, e.g. '10 kN'; SENB/CT only, conflicts with load_range; '' omits. | |
| mode | No | evaluate, critical or growth; compute stress intensity, solve critical size or integrate crack growth. | evaluate |
| span | No | SENB support span S, e.g. '400 mm'; requires S/W=4, unused by other geometries; '' omits. | |
| width | No | Full plate width W or specimen width, e.g. '100 mm'; all geometries except infinite require it; '' omits. | |
| stress | No | Remote maximum tensile stress, e.g. '100 MPa'; plate geometries, conflicts with stress_range; '' omits. | |
| geometry | No | infinite, center_secant, center_tada, edge_small, edge, double_edge, surface, senb or ct; see geometry limits in docs. | infinite |
| growth_c | No | Paris/Forman C with composite units, e.g. '1e-12 m/cycle/(MPa*m^0.5)^3'; growth only; see Forman units. | |
| growth_m | No | Paris/Forman power m, dimensionless .5..8; must agree with the composite units of C. | |
| thickness | No | Plate/specimen thickness B or t, e.g. '10 mm'; surface/SENB/CT require it, others use for size screen; '' omits. | |
| threshold | No | No-growth Delta_K threshold, e.g. '4 MPa*m^0.5'; growth only; '' means zero threshold. | |
| toughness | No | Mode-I toughness Kc or KIc, e.g. '50 MPa*m^0.5'; required critical/Forman, optional evaluate/Paris; '' omits. | |
| crack_size | No | Initial crack depth a or central half-length, e.g. '2 mm'; required in evaluate/growth, optional critical; '' omits. | |
| growth_law | No | paris or forman; Forman requires Kc and its own dimensionally different coefficient C. | paris |
| load_range | No | Force range Delta_P, e.g. '5 kN'; growth SENB/CT only, max=range/(1-R); '' omits. | |
| load_ratio | No | Growth stress ratio R=Kmin/Kmax, dimensionless 0..0.95, default 0; compressive cycles are outside scope. | |
| final_crack | No | Growth end limit a_f, e.g. '10 mm'; '' uses critical size, explicit limit is capped by Kc instability. | |
| stress_range | No | Remote stress range Delta_sigma, e.g. '50 MPa'; growth plates only, max=range/(1-R); '' omits. | |
| table_points | No | Growth CSV stations, 2..101, default 31; log-spaced crack lengths, cumulative cycles. | |
| surface_point | No | deepest or surface point for Newman-Raju; both K values are reported, selected point controls growth. | deepest |
| yield_strength | No | Yield stress for LEFM screens, e.g. '400 MPa'; optional, peak net-section stress above .8 yield is refused; '' omits. | |
| surface_half_length | No | Surface half-length c, e.g. '5 mm'; surface only, paired with initial a; growth holds a/c fixed; '' omits. | |
| integration_tolerance | No | Relative life tolerance for integration and critical endpoint, 1e-10..1e-3, default 1e-7; cap 50000 evaluations. |